Is there any one who can teach me how to controll the below quality demand regarding roller wave while tempering
thickness vs. roller wave
3 mm 0.30 mm
4 mm 0.15 mm
6~12 mm 0.10 mm
13~16 mm 0.05 mm
Thanks,
Tony
I have read and I agree to glassonweb.com's Terms of Use, including Privacy Policy and Cookie Use.
On
Greetings from Strainoptics. Please be advised that Strainoptics Inc.(USA)offers equipment for measuring roller wave and optical distortion. Please contact us at stress@strainoptics.com or visit our website www.strainoptics.com.
Kind Regards
Barbara Hoffman
Strainoptics Inc
Tel ++ 215-661-0100 ext. 102
Fax ++ 215-699-7028