Glass lamination temperature and pressure settings in Autoclave

Can any one describe the details for the autoclave pressure and temperature settings for different thickness. Share any links or related articles for the same. We are now working with 12.5 bar pressure and 135 degree temperature ,hold time 100 minutes. By this setting is running good with 6mm glass. But by this setting 12 mm thickness is getting bubbles.I am thanking in advance for share any suggestions

Roby Englaro
Sat, 20/08/2022 - 10:39

With 12mm glass you need longer heating time, because the mass is double. In any case your PVB supplier knows very well which are the best settings for your autoclave.

I have read and I agree to glassonweb.com's Terms of Use, including Privacy Policy and Cookie Use.